GH-2217
|
200℃/10'
|
64
|
6-7
|
32-38
|
3800-4800
|
Good flow and good weathering resistance
|
|
|
GH-2219△
|
200℃/10'
|
65
|
8
|
31-37
|
3300-4300
|
Outstanding flow and good heat endurance property
|
|
|
GH-2224
|
200℃/10'
|
62
|
7
|
29-35
|
2800-4800
|
Good flow and gas-oven resistance;good mechanical property
|
|
|
GH-2270
|
200℃/10'
|
64
|
6-7
|
32-38
|
4500-5500
|
Balanced weathering resistance;excellent after-process performance
|
|
|
GH-2230
|
160℃/10'
|
62
|
5
|
32-38
|
3000-4500
|
Low temperature fast curing; good mechanical property
|
|
|
GH-2235
|
200℃/10'
|
56
|
6
|
31-37
|
5500-6500
|
Excellent flexibility; good flow and mechanical property
|
|
|
GH-2236
|
200℃/10'
|
64
|
7
|
30-36
|
3800-4800
|
Excellent flow and weathering resistance
|
|
|